Precipitaion Hardening Stainless hlau
Kub Kub Alloy
◆0Cr17Ni7Al yog cov nag lossis daus-tawv hlau nrog Al ntxiv, siv los ua cov springs, ntxhua khaub ncaws, tshuab xam zauv, thiab lwm yam.
◆0Cr15Ni7Mo2Al yog siv rau cov thawv muaj zog, qhov chaw thiab cov khoom siv nrog qee yam kev tiv thaiv corrosion.
◆ Kev ua tau zoo ntawm 0Cr15Ni5Cu4Nb zoo ib yam li 0Cr17Ni4Cu4Nb, tab sis nws muaj kev ua haujlwm zoo dua.
◆0Cr12Mn5Ni4Mo3Al (Gangyan 69111) muaj cov yas zoo dua li 0Cr15Ni7Mo2Al.
◆0Cr17Ni4Cu4Nb Precipitation hardening steel nrog Cu ntxiv, dav siv nyob rau hauv shafts, high-strength structural yam uas yuav tsum tau corrosion kuj rau chav turbine qhov chaw.
◆ XM -25 yog kub thiab kub resistant, haum rau roj av, tshuaj, aerospace, nuclear zog thiab lwm yam lag luam.
Tshuaj muaj pes tsawg leeg
Qib | C | Si | Mn | S | P | Cr | Ni | Mo | Cu | Nb | Al | lwm yam |
tsis muaj ntau dua | ||||||||||||
0Cr17Ni4Cu4 Nb | 0.07 ib | 1 | 1 | 0.035 ib | 0.03 ib | 15.5-17.5 Nws | 3 x5 | - | 3 x5 | 0.15–0.45 dr hab | - | - |
0Cr17Ni7Al | 0.09 ib | 1 | 1 | 0.035 ib | 0.03 ib | 16-18 : kuv | 6.5-7.5 hli | - | ≤0.5 | - | 0.75-1.5 hli | - |
0Cr15Ni7Mo2Al | 0.09 ib | 1 | 1 | 0.035 ib | 0.03 ib | 14-16 | 6.5-7.75 Nws | 2 ~3 | - | - | 0.75-1.5 hli | - |
0Cr15Ni5Cu4 Nb | 0.07 ib | 1 | 1 | 0.035 ib | 0.03 ib | 14-15.5 Nws | 3.5 ~ 5.5 hli | - | 2.5 ~ 4.5 hli | 5 * C% ~ 0.45 | - | - |
0Cr12Mn5Ni4Mo3Al | 0.09 ib | 0.8 ua | 4.4-5.3 | 0.03 ib | 0.03 ib | 11 ~ 12 | 4x 5 | 2.7-3.3 | - | - | 0.5 ~ 1 | - |
XM-25 | 0.05 Nws | 1 | 1 | 0.03 ib | 0.03 ib | 14-16 | 5 x7 | 0.5 ~ 1 | 1.25-1.75 Nws | ≥8 * C% | - | - |
Alloy khoom yam tsawg kawg nkaus
Qib | xeev | tensile zog RmN/m ㎡ | Yield zog Rp0.2N/m㎡ | Elongation li% | HRC (HBS) |
0Cr17Ni7Al | Cov tshuaj 1000 ~ 1100 ℃ ceev txias | ≤1030 | ≤380 | ≥ 20 | ≤ 229 |
565 ℃ kev laus | ≥1140 | ≥960 | ≥5 | ≥363 | |
510 ℃ kev laus | ≥1230 | ≥1030 | ≥4 | ≥388 | |
0Cr17Ni4Cu4 Nb | 480 ℃ kev laus | ≥1310 | ≥1180 | ≥10 | ≥40 |
550 ℃ kev laus | ≥1060 | ≥1000 | ≥12 | ≥35 | |
580 ℃ kev laus | ≥1000 | ≥865 | ≥13 | ≥31 | |
620 ℃ kev laus | ≥930 | ≥325 | ≥16 | ≥ 28 | |
0Cr15Ni5Cu4 Nb | kev daws teeb meem | - | - | - | ≤380 |
565 ℃ kev laus | ≥1210 | ≥1100 | ≥7 | ≥375 | |
510 ℃ kev laus | ≥1320 | ≥1210 | ≥6 | ≥388 | |
0Cr12Mn5Ni4Mo3Al | 520 ℃ kev laus | ≥1520 | ≥1280 | ≥9 | ≥47 |
XM-25 | 560 ℃ kev laus | ≥1100 | ≥1000 | ≥10 | ≥45 |