Hastelloy C-276 Cov Ntaub Ntawv Cov Ntaub Ntawv
Product Description
HT PIPE muab Hastelloy C276 Nickel alloy round bar, Alloy C276 Bar tsum nyob rau hauv Suav teb.2.4819 round bar, Alloy C276 pas nrig, UNS N10276 pas nrig, Alloy C276 tiaj Bar, Hastelloy C276 hollow bar, Hastelloy C276 Nickel alloy round bar tsum, exporter.
Dab tsi yog cov yam ntxwv ntawm Hastelloy C276?
● Zoo heev corrosion kuj nyob rau hauv txo ib puag ncig
● Exceptional tiv thaiv rau muaj zog daws ntawm oxidizing ntsev, xws li ferric thiab cupric chlorides
● High nickel thiab molybdenum cov ntsiab lus muab kev tiv thaiv corrosion zoo hauv kev txo qis ib puag ncig
● Cov ntsiab lus tsis tshua muaj carbon tsawg uas txo qis cov qoob loo ntawm ciam teb carbide nag lossis daus thaum lub sij hawm vuam kom muaj kev tiv thaiv corrosion nyob rau hauv tshav kub-cuam tshuam cheeb tsam ntawm welded pob qij txha
● Resistance to localized corrosion xws li pitting thiab stress-corrosion cracking
● Ib qho ntawm ob peb cov ntaub ntawv los tiv thaiv corrosive los ntawm cov roj chlorine ntub dej, hypochlorite thiab chlorine dioxide
Hastelloy C276 Nickel alloy round bar tshuaj muaj pes tsawg leeg,%
Ni | Mo | Cr | Fe | W | Co | Mn | C | V | P | S | Si |
Tseem tshuav | 15.0-17.0 Nws | 14.5-16.5 Nws | 4.0-7.0 Nws | 3.0-4.5 | 2.5 max | 1.0 max | 01 max | 35 max | 04 max | 03 max | 08 max |
Specifications
ASTM Cov Lus Qhia
cev Smls | Cov yeeb nkab Welded | Tube Smls | Tube Welded | Ntawv / phaj | Bar | Forging | Haum | Hlau |
B622 | b619 ua | B622 | B626 | b575 ua | b574 ua | b564 ua | B366 |
Hastelloy C276 Lub cev muaj zog
Melting point: 1325-1370 ℃
Qhov ceev: 8.90 g / cm3
Alloy C276 Bar Mechanical Properties
Mechanical zog | Tensile, min, ksi [MPa] | Yield, min, ksi [MPa] | Elongation,% (min) |
Hastelloy C276 | 100 [690] | 41 [283] | 40 |
Hom Chav Kub Kub Tensile Properties ntawm Annealed Material
Daim ntawv khoom | Tensile (ksi) | .2% Yield (ksi) | Elongation% |
Bar | 110.0 Nws | 52.6 ib | 62 |
Phaj | 107.4 ib | 50.3 | 67 |
Daim ntawv | 115.5 ib | 54.6 ib | 60 |
Tube & Yeeb | 105.4 ib | 45.4 ib | 70 |