  • 17-4PH Cov Ntaub Ntawv Cov Ntaub Ntawv

    International identifiers

    AISI 630, ASTM A564-89 17-4PH, JIS SCS24 / SUS630, AFNOR Z7CNU15-05 / Z7CNU17-04

  • Precipitaion Hardening Stainless hlau

    Kev kub siab Alloy Chemical muaj pes tsawg leeg Qib C Si Mn SP Cr Ni Mo Cu Nb Al lwm yam tsis ntau dua 0Cr17Ni4Cu4Nb 0.07 1 1 0.035 0.03 15.5 ~ 17.5 3~5 - 3~5 0.15 15 Cr. 1 0.035 0.03 16~18 6.5~7.5 - ≤0.5 - 0.75~1.5 - 0Cr15Ni7Mo2Al 0.09 1 1 0.035 0.03 14~16 6.5~7.75 2~3 - - 0.75b.70C1 .035 0.03 14 ~ 15.5 3.5~...