MONEL npib tsib xee-tooj liab alloy 400 (UNS N04400) yog ib qho kev daws teeb meem uas tuaj yeem ua kom tawv nqaij xwb los ntawm kev ua haujlwm txias.Nws muaj lub zog siab thiab toughness nyob rau hauv ntau qhov kub thiab txias thiab ua haujlwm zoo rau ntau qhov chaw corrosive.Alloy 400 yog dav siv nyob rau hauv ntau lub teb, tshwj xeeb tshaj yog marine thiab tshuaj ua.Cov kev siv ib txwm yog li qub thiab twj tso kua mis;twj tso kua mis thiab kiv cua shafts;marine fixtures thiab fasteners;cov khoom siv hluav taws xob thiab hluav taws xob;springs;Cov khoom siv tshuaj ua haujlwm;roj av thiab dej tshiab tank;cov roj av tsis zoo, cov hlab ntsha thiab cov kav dej;boiler pub dej rhaub thiab lwm yam kub exchangers;thiab deaerating heaters.Chemical Compositions