IInconel
Kub Kub Alloy
◆Inconel600 (N06600) muaj corrosion kuj rau ntau yam corrosive xov xwm, nws kuj muaj zoo creep rupture zog, pom zoo rau qhov chaw ua hauj lwm hauv qab no 700 ℃.Nws yog tsuas yog siv nyob rau hauv kev tsim khoom thiab siv cov corrosive alkali hlau, tshwj xeeb tshaj yog nyob rau hauv ib puag ncig uas siv sulfides.
◆ Ib qho tseem ceeb ntawm Inconel601 (N06601) yog tias nws muaj oxidation tsis kam thiab zoo carbonization tsis kam thaum kub siab li 1180 ° C. Nws yog tsuas yog siv nyob rau hauv kev kho cua sov ua qhov chaw, pa system qhov chaw, thiab oxygen reheaters.
◆Inconel625 (N06625Ns336) nthuav tawm zoo heev corrosion kuj nyob rau hauv ntau yam xov xwm, thiab cov mos mos annealed low-carbon alloy 625 yog dav siv nyob rau hauv cov txheej txheem tshuaj, qhov twg nws tiv nrog seawater thiab withstands siab mechanical stress.
◆Inconel725 muaj zog corrosion kuj thiab yog haum rau cov yeeb nkab fittings thiab marine nkoj.
◆ Inconel690 muaj anti-oxidation thiab anti-corrosion zog, thiab yog haum rau petrochemical, metallurgy, nuclear zog, thiab lwm yam.
Tshuaj muaj pes tsawg leeg
Qib | C | Si | Mn | S | P | Cr | Ni | Fe | Al | Ti | Cu | Mo | Nb | lwm yam |
tsis muaj ntau dua | ||||||||||||||
Inconel 600 | 0.15 | 0.5 | 1 | 0.015 ib | 0.03 ib | 14-17 ib | puag | 6-10 | - | - | ≤0.5 | - | - | - |
Inconel 601 | 0.1 | 0.5 | 1 | 0.015 ib | 0.03 ib | 21-25 ib | puag | 10 ~ 15 | 1-1.7 | - | ≤1 | - | - | - |
Inconel 625 | 0.1 | 0.5 | 0.5 | 0.015 ib | 0.015 ib | 20-23 | puag | ≤ 5 | ≤0.4 | ≤0.4 | - | 8-10 | 3.15–4.15 dr hab | Co≤1 |
Inconel725 | 0.03 ib | 0.2 | 0.35 Nws | 0.01 ib | 0.015 ib | 19-22.5 Nws | 55-59 ib | Nyob twj ywm | 0.35 Nws | 1-1.7 | — | 7 ;9,5 | 2.75-4 | - |
Inconel 690 | 0.05 Nws | 0.5 | 0.5 | 0.015 ib | 0.03 ib | 27-31 ib | ≥58 | 7-11 | — | — | ≤0.5 | — | — | - |
Alloy khoom yam tsawg kawg nkaus
Qib | alloy lub xeev | tensile zog RmN/m ㎡ | Yield zog Rp0.2N/m㎡ | Elongation li% | Brinell hardness HB |
Inconel 600 | Kev kho mob | 550 | 240 | - | ≤195 |
Kev kho mob | 500 | 180 | - | ≤185 | |
Inconel 601 | Annealing | 650 | 300 | - | - |
Kev kho mob | 600 | 240 | - | ≤ 220 | |
Inconel 625 | Kev kho mob | 760 ib | 345 | - | ≤ 220 |
Inconel725 | Kev kho mob | 790 ua | 485 ib | 28 | - |
Inconel 690 | Kev kho mob | 780 ua | 450 | 25 | - |