Kev nthuav qhia lub zog ntawm Hastelloy C-276

At Hangnie Super Alloys Co., Ltd., peb nkag siab txog lub luag haujlwm tseem ceeb ntawm cov ntaub ntawv ua tau zoo ua si hauv ntau yam kev lag luam. Niaj hnub no, peb yuav delve rau hauv cov khoom tshwj xeeb thiab cov txheej txheem tsim khoom ntawmHastelloy C-276, nickel-alloy puag ncig bar muaj npe nrov rau nws qhov tshwj xeeb tiv thaiv corrosion.

Tsis sib haum Corrosion Resistance:

Hastelloy C-276 sawv tawm rau nws qhov kev tsis sib haum xeeb rau ntau qhov chaw corrosive. Nov yog saib ze dua ntawm nws qhov tseem ceeb lub zog:

Kev Loj Hlob hauv Kev Txo Cov Ib puag ncig: Cov hlau no ua tau zoo nyob rau hauv ib puag ncig uas tshem tawm cov pa oxygen, ua rau nws zoo tagnrho rau ntau yam kev siv tshuaj lom neeg.

Conquers Strong Oxidizing Salt Solutions: Hastelloy C-276 tackles aggressive solutions uas muaj ferric thiab cupric chlorides yooj yim.

Nickel & Molybdenum Powerhouse: Cov ntsiab lus siab ntawm cov ntsiab lus no tiv thaiv cov hlau tiv thaiv corrosion hauv kev txo qis ib puag ncig.

Tsawg Carbon Advantage: Tsawg cov ntsiab lus carbon tiv thaiv cov qoob loo ntawm cov ciam teb carbide nag lossis daus thaum lub sijhawm vuam, ua kom muaj kev tiv thaiv corrosion hauv cov cheeb tsam welded.

Localized Corrosion Foe: Cov khoom no muaj txiaj ntsig zoo tiv thaiv kev tawm tsam hauv zos xws li pitting thiab kev ntxhov siab-corrosion tawg.

Champion Against Chlorine Challenges: Ib qho ntawm ob peb alloys uas tuaj yeem tiv taus qhov hnyav ntawm cov roj chlorine ntub dej, hypochlorite, thiab chlorine dioxide.

Hastelloy C-276: Lub cev muaj zog ntawm ib sab

Melting Point: 1325-1370 ° C (High melting point qhia tshwj xeeb tiv thaiv rau qhov kub thiab txias)

Ceev: 8.90 g / cm3 (High ceev pab txhawb rau cov khoom lub zog thiab durability)

Cov Txheej Txheem Ntau Lawm (Ceeb Toom: Cov ntsiab lus tshwj xeeb yuav txawv nyob ntawm tus neeg tsim khoom)

Thaum cov txheej txheem ntau lawm yuav txawv me ntsis ntawm cov tuam txhab, ntawm no yog ib qho kev qhia dav dav ntawm Hastelloy C-276 round bars feem ntau tsim:

Melting: Cov ntaub ntawv raw, xws li npib tsib xee, molybdenum, chromium, tungsten, thiab hlau nyob rau hauv cov proportions meej, yog melted nyob rau hauv lub nqus induction rauv (VIM) los yog ib tug ua ke ntawm VIM thiab electroslag remelting (ESR) kom purity thiab tshem tawm impurities.

Casting: Cov hlau molten yog tom qab ntawd nchuav rau hauv pwm los tsim cov ingots ntawm qhov xav tau loj thiab cov duab.

Kev Ua Haujlwm Kub Kub: Cov ingots raug rau cov txheej txheem ua haujlwm kub xws li forging lossis extrusion kom ua tiav cov duab xav tau thiab txhim kho cov khoom ntawm cov qauv nplej thiab cov khoom siv tshuab.

Kev kho cua sov: Cov txheej txheem kev kho cua sov tau siv los ua kom cov txheej txheem ua kom zoo dua qub thiab ua kom zoo dua cov khoom siv tiv thaiv corrosion thiab lub zog txhua yam.

Surface Finishing: Cov kauj ruam kawg suav nrog cov txheej txheem txheej txheej zoo li machining, sib tsoo, lossis polishing kom ua tiav qhov xav tau ntawm qhov chaw tiav thiab qhov ntev ntev.

Kev Tswjhwm Zoo: Cov kev tswj xyuas nruj nruj tau ua tiav thoob plaws hauv cov txheej txheem tsim khoom kom ntseeg tau tias cov tuav tau ua tau raws li tag nrho cov txheej txheem tshuaj lom neeg, cov khoom siv kho tshuab, thiab qhov yuav tsum tau muaj.

Hangnie Super Alloys: Koj Trusted Partner rau Hastelloy C-276

Ntawm Hangnie Super Alloys Co., Ltd., peb tau cog lus los muab peb cov neeg siv khoom zoo tshaj plaws Hastelloy C-276 round bars. Peb cov kws tshaj lij hauv kev xaiv cov khoom siv, cov txheej txheem tsim khoom, thiab kev tswj xyuas kom zoo ua kom koj tau txais cov khoom lag luam uas muab kev ua tau zoo tshaj plaws thiab kev ua haujlwm ntev nyob rau hauv qhov chaw xav tau tshaj plaws.

Yog xav paub ntxiv lossis xav paub ntxiv txog yuav ua li cas Hastelloy C-276 tuaj yeem muaj txiaj ntsig zoo rau koj cov ntawv thov tshwj xeeb, thov hu rau dawbtiv tauj pebhnub no.