Unveiling the Robustness of SUPER DUPLEX 2507

Nyob rau hauv lub realm ntawm high-kev ua tau zoo cov ntaub ntawv,Hangnie Super Alloys Co., Ltd.sawv ntawm forefront, nthuav qhia covSUPER DUPLEX 2507- ib tug super duplex stainless hlau uas epitomizes lub zog thiab corrosion kuj. Engineered rau cov ntawv thov tshaj plaws, cov hlau no yog ib qho pov thawj rau lub tuam txhab kev cog lus rau kev ua tau zoo.

Kev sib xyaw thiab kev ua haujlwm

SUPER DUPLEX 2507 yog kev sib haum xeeb ntawm 25% chromium, 4% molybdenum, thiab 7% npib tsib xee. Qhov kev sib xyaw ua ke no ua kom muaj kev tiv thaiv zoo rau chloride pitting thiab crevice corrosion, ua tsaug rau nws cov molybdenum siab, chromium, thiab nitrogen cov ntsiab lus. Lub duplex qauv ntawm cov alloy imparts nws nrog ib tug tshwj xeeb tsis kam mus rau chloride kev nyuaj siab corrosion cracking, ua rau nws ib tug txhim khu kev qha kev xaiv rau ib puag ncig tseem ceeb.

Mechanical Properties thiab Applications

Nrog nws cov khoom siv zoo tshaj plaws, SUPER DUPLEX 2507 feem ntau tso cai rau kev siv cov khoom siv sib zog kom ua tiav qhov tsim qauv zoo ib yam li cov hlau npib tsib xee tuab. Qhov kev txo qhov hnyav no txhais ua kev txuag nqi tseem ceeb hauv kev tsim khoom. Lub alloy tus nqi qis ntawm thermal expansion thiab zoo weldability thiab workability ntxiv txhim khu nws kev thov nyob rau hauv ntau yam lag luam.

Optimal Siv thiab txwv

Thaum lub alloy qhov kev ua tau zoo yog qhov tsis lees paub, nws raug pom zoo kom txwv nws qhov kev siv rau qhov kub qis dua 600 ° F (316 ° C). Lub sij hawm ntev raug rau qhov kub siab dua tuaj yeem cuam tshuam nws qhov toughness thiab corrosion kuj.

Cov ntawv thov kev lag luam

SUPER DUPLEX 2507 pom nws qhov chaw hauv ntau daim ntawv thov, suav nrog:

• Desalination Equipment: Nws tiv taus cov chloride-nplua nuj ib puag ncig ua rau nws zoo tagnrho rau cov chaw kho dej.

• Cov txheej txheem tshuaj lom neeg lub siab, cov kav dej, thiab cov khoom siv hluav taws xob kub: Cov hlau tiv taus qhov hnyav ntawm kev ua tshuaj lom neeg.

• Kev siv dej hiav txwv: Lub hiav txwv corrosive tsis sib xws rau 2507's robustness.

• Cov Khoom Siv Hluav Taws Xob Hluav Taws Xob: Nws ua tau zoo hauv kev tawm tsam cov kua qaub thiab cov tshuaj chloride-laden ib puag ncig ntawm cov tshuab ntxhua khaub ncaws.

• Pulp & Paper Mill Equipment: Resisting cov organic acids tam sim no nyob rau hauv cov kev lag luam, lub 2507 ua kom lub neej ntev thiab kev ntseeg tau.

• Offshore Oil Production/Technology and Oil and Gas Industry Equipment: Lub alloy lub zog thiab corrosion kuj tseem ceeb heev nyob rau hauv cov huab cua ntawm cov roj thiab roj extraction.

Xaus

Hangnie Super Alloys Co., Ltd. muaj kev txaus siab los muab SUPER DUPLEX 2507, ib yam khoom uas tsis yog tsuas yog ua tau raws li tab sis tshaj cov qauv kev lag luam rau kev ua haujlwm ntev thiab kev ua haujlwm. Raws li ib tus neeg muab kev ntseeg siab, Hangnie ua kom ntseeg tau tias txhua lub lens qhia txog qhov kawg ntawm kev tsim kho tshiab hauv stainless hlau thev naus laus zis.

Yog koj txaus siab thovtiv tauj peb:

Email:andrew@hnsuperalloys.com

WhatsApp: +86 13661794406

SUPER DUPLEX 2507 Zoo siab


Post lub sij hawm: Apr-15-2024