Monel
Kub Kub Alloy
◆ Monel400 muaj kev tiv thaiv corrosion zoo heev hauv hydrofluoric acid thiab fluorine roj, thiab yog tsim rau cov yeeb nkab fittings thiab li qub siv hauv kev lag luam tshuaj, roj av, atomic zog, thiab kev tsim kho marine.
◆ Monel500 muaj cov cuab yeej zoo txhua yam, lub zog siab thiab zoo corrosion kuj. Nws yog tsim rau fasteners thiab cov khoom siv hauv kev lag luam chemical, nkoj thiab marine engineering.
◆ Monel404 yog siv dav hauv kev lag luam petrochemical, nuclear kev lag luam, thiab lwm yam kev lag luam kev lag luam.
Tshuaj muaj pes tsawg leeg
Qib | C | Si | Mn | S | P | Cr | Ni | Mo | Fe | Co | W | Al | Ti | Cu |
tsis muaj ntau dua | ||||||||||||||
Monel 400 | 0.3 | 0.5 | 2 | 0.024 ib | - | - | puag | - | ≤ 2.5 | - | - | - | - | 28-34 ib |
Monel 500 | 0.18 | 0.5 | 1.5 | 0.01 ib | - | - | ≥63 | - | ≤ 2 | - | - | 2.3-3.15 Nws | 0.35-0.85 Nws | 27-33 ib |
Monel404 | 0.15 | 0.1 | 0.1 | 0.024 ib | - | - | 52-57 ib | - | ≤0.5 | - | - | ≤ 0.05 | - | Nyob twj ywm |
Alloy khoom yam tsawg kawg nkaus
Qib | Tej yam kev mob | tensile zog RmN/m ㎡ | Yield zog Rp0.2N/m㎡ | Elongation li% | Brinell hardness HB |
Monel 400 | Forged / kub dov | 516 | 170 | 35 | - |
Annealed xeev | 483 ib | 170 | 35 | - | |
Monel 500 | Forged xeev + laus | 960 ua | 686 ib | 20 | 27 |
kev daws teeb meem + kev laus | 896 ib | 585 ib | 20 | 24 | |
Monel404 | Annealed xeev | 550 | 185 | 36 | - |