Inconel

  • IInconel

    High Temperature Alloy Chemical composition Grade C Si Mn SP Cr Ni Fe Al Ti Cu Mo Nb lwm yam tsis muaj ntau tshaj Inconel600 0.15 0.5 1 0.015 0.03 14~17 puag 6~10 - - ≤0.5 - - - Inconel601. 1.3~ 10. 25 puag 10~15 1~1.7 - ≤1 - - - Inconel625 0.1 0.5 0.5 0.015 0.015 20~23 base ≤5 ≤0.4 ≤0.4 - 8~10 3.15~ 5con.30.14. 0...